hpulcas is an acronym for High Purity Ultra Low Carbon and Sulfur.
hpulcas GmbH has developed and implemented a new process to fabricate high purity nickel. The new grade of hpulcas nickel with a purity of 99.98 % meets and surpasses the requirements for Ni 270. The key to the process is the use of high purity cathode plates instead of nickel powder or melt metallurgy. The cathode plates are hot rolled to a uniform 6 mm, levelled, brushed, cut to rectangular format and joined by welding. The strip thus manufactured is then rolled down to the required thickness by cold rolling and interim annealing. The high degree of purity results in special and reproducible properties, which are used in demanding applications ranging from temperature sensors and controls, welding and brazing products, battery and supercapacitor components, diffusion barriers in roll bonded clad metals, contacts and thermobimetals. The products include sheets, strips, foil, coil and wire. A wide range of dimension and mechanical and surface properties can be provided.
Sitio web
Ingresos
0-1M EUR
Número de empleados
11-50
Año de creación
2011
Tipo
Manufacturer, Processor and Distributor
Patentes
2
Certificados de calidad
Our quality management system is certified according to ISO 9001: 2015.
Certifications
ISO 9001
High Purity Nickel Products
Metalurgia
Non-Ferrous Products
Componentes electrónicos
Electronic Components Others
Electrónica
Energía
Fabricación
Tratamiento de superficies y revestimiento
Alambres y cables
Baterías
Battery Contacts
Blanco de pulverización
Celdas de combustible
Contactos eléctricos
Electrochemical Machines
Equipos de cizallamiento
Ingeniería eléctrica
Lithium-Ion Batteries
Sensores
Solid Oxide Fuel Cells (Sofc)
Industria de materiales compuestos
Metal Laminate Composite
Nickel Based Composite
Pulverización térmica
Accesorios eléctricos
Actuadores
Automotriz
Bonding
Capacitors In General
Coating Material Additives
Componentes para equipos eléctricos
Condensadores
Diffusion Bonding
Dispositivos semiconductores
Electrodos
Enchufes
Equipamiento para la industria del vidrio y la cerámica
Equipment For Glass Making
Filamentos
High Purity Nickel Flat Wire & Ribbon
High Purity Nickel Wire & Rods
Juntas
Motores de combustión
Motores de combustión interna
Other Capacitors
Other Semiconductor Devices
Piezas generales para vehículos
Processes In The Glass & Ceramics Industries
Roll Bonding
Sistemas de control
Sistemas mecánicos
Soldadura
Soldadura y soldadura fuerte
Supercapacitor
Terminales eléctricas
Vidrio y cerámica
Grade | Shape | ||
---|---|---|---|
EN 2.4050 | Plate, Strip, Foil, Rod, Wire | EN 2.4050, UNS N02270, DIN 2.4050, UNS N02200, UNS N02201, DIN 2.4060, EN 2.4060, DIN 2.4061, EN 2.4061, DIN 2.4066, EN 2.4066, DIN 2.4068, EN 2.4068, UNS N02205 | |