Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Bario | 2E-6 % Show Supplier Material materials with Bario of 2E-6 % |
Boro | 1.5E-5 % Show Supplier Material materials with Boro of 1.5E-5 % |
Calcio | 7E-6 % Show Supplier Material materials with Calcio of 7E-6 % |
Circonio | 5E-6 % Show Supplier Material materials with Circonio of 5E-6 % |
Cromo | 5E-6 % Show Supplier Material materials with Cromo of 5E-6 % |
Fósforo | 5E-5 % Show Supplier Material materials with Fósforo of 5E-5 % |
Galio | 2E-6 % Show Supplier Material materials with Galio of 2E-6 % |
Hierro | 5E-5 % Show Supplier Material materials with Hierro of 5E-5 % |
Magnesio | 5E-5 % Show Supplier Material materials with Magnesio of 5E-5 % |
Manganeso | 5E-6 % Show Supplier Material materials with Manganeso of 5E-6 % |
Níquel | 5E-6 % Show Supplier Material materials with Níquel of 5E-6 % |
Plata | 5E-6 % Show Supplier Material materials with Plata of 5E-6 % |
Plomo | 5E-6 % Show Supplier Material materials with Plomo of 5E-6 % |
Silicona | 5E-5 % Show Supplier Material materials with Silicona of 5E-5 % |
Titanio | 1E-5 % Show Supplier Material materials with Titanio of 1E-5 % |
Vanadio | 1E-5 % Show Supplier Material materials with Vanadio of 1E-5 % |