Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Antimonio | 8E-6 % Show Supplier Material materials with Antimonio of 8E-6 % |
Arsénico | 5E-6 % Show Supplier Material materials with Arsénico of 5E-6 % |
Azufre | 1E-5 % Show Supplier Material materials with Azufre of 1E-5 % |
Bario | 2E-6 % Show Supplier Material materials with Bario of 2E-6 % |
Berilio | 1E-6 % Show Supplier Material materials with Berilio of 1E-6 % |
Bismuto | 5E-6 % Show Supplier Material materials with Bismuto of 5E-6 % |
Boro | 2E-6 % Show Supplier Material materials with Boro of 2E-6 % |
Calcio | 4E-6 % Show Supplier Material materials with Calcio of 4E-6 % |
Cerio | 1E-5 % Show Supplier Material materials with Cerio of 1E-5 % |
Cesio | 5E-6 % Show Supplier Material materials with Cesio of 5E-6 % |
Circonio | 3E-6 % Show Supplier Material materials with Circonio of 3E-6 % |
Cloro | 1E-5 % Show Supplier Material materials with Cloro of 1E-5 % |
Cobalto | 1E-6 % Show Supplier Material materials with Cobalto of 1E-6 % |
Cobre | 1E-5 % Show Supplier Material materials with Cobre of 1E-5 % |
Cromo | 4E-6 % Show Supplier Material materials with Cromo of 4E-6 % |
Estaño | 5E-6 % Show Supplier Material materials with Estaño of 5E-6 % |
Flúor | 1E-5 % Show Supplier Material materials with Flúor of 1E-5 % |
Fósforo | 3E-5 % Show Supplier Material materials with Fósforo of 3E-5 % |
Galio | 1E-6 % Show Supplier Material materials with Galio of 1E-6 % |
Germanio | 1E-5 % Show Supplier Material materials with Germanio of 1E-5 % |
Hierro | 1E-5 % Show Supplier Material materials with Hierro of 1E-5 % |
Indio | 5E-6 % Show Supplier Material materials with Indio of 5E-6 % |
Lantano | 6E-6 % Show Supplier Material materials with Lantano of 6E-6 % |
Litio | 1E-6 % Show Supplier Material materials with Litio of 1E-6 % |
Magnesio | 1.5E-5 % Show Supplier Material materials with Magnesio of 1.5E-5 % |
Manganeso | 2E-6 % Show Supplier Material materials with Manganeso of 2E-6 % |
Molibdeno | 2E-6 % Show Supplier Material materials with Molibdeno of 2E-6 % |
Níquel | 5E-6 % Show Supplier Material materials with Níquel of 5E-6 % |
Plata | 5E-6 % Show Supplier Material materials with Plata of 5E-6 % |
Platino | 1E-5 % Show Supplier Material materials with Platino of 1E-5 % |
Plomo | 5E-6 % Show Supplier Material materials with Plomo of 5E-6 % |
Silicona | 1E-5 % Show Supplier Material materials with Silicona of 1E-5 % |
Sodio | 5E-6 % Show Supplier Material materials with Sodio of 5E-6 % |
Thorium | 1E-6 % Show Supplier Material materials with Thorium of 1E-6 % |
Titanio | 5E-6 % Show Supplier Material materials with Titanio of 5E-6 % |
Uranio | 1E-6 % Show Supplier Material materials with Uranio of 1E-6 % |
Vanadio | 1E-5 % Show Supplier Material materials with Vanadio of 1E-5 % |
Wolframio | 5E-6 % Show Supplier Material materials with Wolframio of 5E-6 % |
Zinc | 5E-6 % Show Supplier Material materials with Zinc of 5E-6 % |