Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Bario | 1E-5 % Show Supplier Material materials with Bario of 1E-5 % |
Boro | 1E-5 % Show Supplier Material materials with Boro of 1E-5 % |
Calcio | 2E-5 % Show Supplier Material materials with Calcio of 2E-5 % |
Circonio | 2E-5 % Show Supplier Material materials with Circonio of 2E-5 % |
Cromo | 1E-5 % Show Supplier Material materials with Cromo of 1E-5 % |
Fósforo | 5E-5 % Show Supplier Material materials with Fósforo of 5E-5 % |
Galio | 1E-5 % Show Supplier Material materials with Galio of 1E-5 % |
Hierro | 2E-5 % Show Supplier Material materials with Hierro of 2E-5 % |
Magnesio | 2E-5 % Show Supplier Material materials with Magnesio of 2E-5 % |
Manganeso | 1E-5 % Show Supplier Material materials with Manganeso of 1E-5 % |
Níquel | 1E-5 % Show Supplier Material materials with Níquel of 1E-5 % |
Plata | 1E-5 % Show Supplier Material materials with Plata of 1E-5 % |
Plomo | 1E-5 % Show Supplier Material materials with Plomo of 1E-5 % |
Silicona | 3E-5 % Show Supplier Material materials with Silicona of 3E-5 % |
Sodio | 5E-5 % Show Supplier Material materials with Sodio of 5E-5 % |
Titanio | 1E-5 % Show Supplier Material materials with Titanio of 1E-5 % |
Vanadio | 2E-5 % Show Supplier Material materials with Vanadio of 2E-5 % |
Zinc | 1E-5 % Show Supplier Material materials with Zinc of 1E-5 % |