Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Antimonio | 1E-6 % Show Supplier Material materials with Antimonio of 1E-6 % |
Arsénico | 1E-6 % Show Supplier Material materials with Arsénico of 1E-6 % |
Azufre | 5E-6 % Show Supplier Material materials with Azufre of 5E-6 % |
Bario | 2E-6 % Show Supplier Material materials with Bario of 2E-6 % |
Berilio | 1E-6 % Show Supplier Material materials with Berilio of 1E-6 % |
Bismuto | 1E-6 % Show Supplier Material materials with Bismuto of 1E-6 % |
Boro | 2E-6 % Show Supplier Material materials with Boro of 2E-6 % |
Calcio | 2E-6 % Show Supplier Material materials with Calcio of 2E-6 % |
Cerio | 1E-6 % Show Supplier Material materials with Cerio of 1E-6 % |
Cesio | 1E-6 % Show Supplier Material materials with Cesio of 1E-6 % |
Circonio | 1E-6 % Show Supplier Material materials with Circonio of 1E-6 % |
Cloro | 1E-6 % Show Supplier Material materials with Cloro of 1E-6 % |
Cobalto | 1E-6 % Show Supplier Material materials with Cobalto of 1E-6 % |
Cobre | 8E-6 % Show Supplier Material materials with Cobre of 8E-6 % |
Cromo | 3E-6 % Show Supplier Material materials with Cromo of 3E-6 % |
Estaño | 1E-6 % Show Supplier Material materials with Estaño of 1E-6 % |
Flúor | 1E-6 % Show Supplier Material materials with Flúor of 1E-6 % |
Fósforo | 1E-5 % Show Supplier Material materials with Fósforo of 1E-5 % |
Galio | 1E-6 % Show Supplier Material materials with Galio of 1E-6 % |
Germanio | 1E-6 % Show Supplier Material materials with Germanio of 1E-6 % |
Hierro | 7E-6 % Show Supplier Material materials with Hierro of 7E-6 % |
Indio | 1E-6 % Show Supplier Material materials with Indio of 1E-6 % |
Lantano | 1E-6 % Show Supplier Material materials with Lantano of 1E-6 % |
Litio | 1E-6 % Show Supplier Material materials with Litio of 1E-6 % |
Magnesio | 8E-6 % Show Supplier Material materials with Magnesio of 8E-6 % |
Manganeso | 2E-6 % Show Supplier Material materials with Manganeso of 2E-6 % |
Molibdeno | 1E-6 % Show Supplier Material materials with Molibdeno of 1E-6 % |
Níquel | 1E-6 % Show Supplier Material materials with Níquel of 1E-6 % |
Plata | 1E-6 % Show Supplier Material materials with Plata of 1E-6 % |
Platino | 5E-6 % Show Supplier Material materials with Platino of 5E-6 % |
Plomo | 1E-6 % Show Supplier Material materials with Plomo of 1E-6 % |
Silicona | 1E-5 % Show Supplier Material materials with Silicona of 1E-5 % |
Sodio | 1E-6 % Show Supplier Material materials with Sodio of 1E-6 % |
Thorium | 1E-8 % Show Supplier Material materials with Thorium of 1E-8 % |
Titanio | 4E-6 % Show Supplier Material materials with Titanio of 4E-6 % |
Uranio | 1E-8 % Show Supplier Material materials with Uranio of 1E-8 % |
Vanadio | 4E-6 % Show Supplier Material materials with Vanadio of 4E-6 % |
Wolframio | 1E-6 % Show Supplier Material materials with Wolframio of 1E-6 % |
Zinc | 1E-6 % Show Supplier Material materials with Zinc of 1E-6 % |