General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.13 g/cm³ Show Supplier Material materials with Densidad of 3.13 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 2244 [-] Show Supplier Material materials with Dureza Vickers of 2244 [-] |
Módulo elástico | 23.0 °C | 420 GPa Show Supplier Material materials with Módulo elástico of 420 GPa |
Resistencia a la compresión | 23.0 °C | 400 MPa Show Supplier Material materials with Resistencia a la compresión of 400 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 74 W/(m·K) Show Supplier Material materials with Conductividad térmica of 74 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components. | |