General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | ISO 62 |
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Dureza Shore D | 85 [-] Show Supplier Material materials with Dureza Shore D of 85 [-] | DIN 53505 | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | min., ISO 527 | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | ISO 527 | |
Hardness, Ball Indentation | 150 MPa Show Supplier Material materials with Hardness, Ball Indentation of 150 MPa | ISO 2039-1 | |
Límite elástico | 66 MPa Show Supplier Material materials with Límite elástico of 66 MPa | ISO 527 | |
Módulo elástico | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | ISO 527 | |
Resistencia a desgarros | 60 kN/m Show Supplier Material materials with Resistencia a desgarros of 60 kN/m | ISO 527 | |
Resistencia a la flexión | 95 MPa Show Supplier Material materials with Resistencia a la flexión of 95 MPa | ISO 178 | |
Resistencia al choque, ensayo Charpy entallado | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | min., ISO 179 | |
Resistencia al choque, ensayo Charpy no entallado | No break, ISO 179 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Coeficiente de dilatación térmica | 8e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8e-05 1/K | DIN 53752 | |
Conductividad térmica | 0.37 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.37 W/(m·K) | DIN 52612 | |
Temperatura máx. de funcionamiento | 100 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 100 °C | Longterm | |
Long | |||
Short | |||
Temperatura mín. de funcionamiento | -40 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -40 °C | Longterm | |
Inflamabilidad | HB UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Rigidez dieléctrica | 50 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 50 kV/mm | VDE 0303 |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | min., VDE 0303 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, rollers and impact stressed parts | |
Certifications | RoHS,REACH |