General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.04 % Show Supplier Material materials with Absorción de agua of 0.04 % | max., ISO 62 |
Coefficient of friction | 0.34 [-] Show Supplier Material materials with Coefficient of friction of 0.34 [-] | DIN 53375, C, Against dry running steel |
Densidad | 1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 78 [-] Show Supplier Material materials with Dureza Shore D of 78 [-] | DIN 53505 |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | min., ISO 527 |
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | ISO 527 |
Hardness, Ball Indentation | 80 MPa Show Supplier Material materials with Hardness, Ball Indentation of 80 MPa | ISO 2039-1 |
Límite elástico | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | ISO 527 |
Módulo elástico | 2 GPa Show Supplier Material materials with Módulo elástico of 2 GPa | ISO 527 |
Resistencia a la flexión | 80 MPa Show Supplier Material materials with Resistencia a la flexión of 80 MPa | ISO 178 |
Resistencia al choque, ensayo Charpy entallado | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 22 kJ/m² | ISO 179 |
Resistencia al choque, ensayo Charpy no entallado | 252 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 252 kJ/m² | ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00015 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00015 1/K | DIN 53752 | |||
Conductividad térmica | 0.13 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.13 W/(m·K) | DIN 52612 | |||
Temperatura de flexión bajo carga | 104 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 104 °C | 2 MPa | |||
145 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 145 °C | 0.45 MPa | ||||
Temperatura de reblandecimiento Vicat | 138 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 138 °C | ISO 306, VST B50 | |||
Temperatura máx. de funcionamiento | 150 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 150 °C | Longterm | |||
Long | |||||
Short | |||||
Temperatura mín. de funcionamiento | -30 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -30 °C | Longterm | |||
Inflamabilidad | V-0 UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Constante dieléctrica | 7 [-] Show Supplier Material materials with Constante dieléctrica of 7 [-] | DIN 53483 |
Rigidez dieléctrica | 27 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 27 kV/mm | VDE 0303 |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | min., VDE 0303 |
Tangente de pérdidas | 0.24 [-] Show Supplier Material materials with Tangente de pérdidas of 0.24 [-] | DIN 53483 |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | min., VDE 0303 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical instruments, pipes and pumps | |
Certifications | RoHS,REACH |