General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.01 % Show Supplier Material materials with Absorción de agua of 0.01 % | max. |
Coefficient of friction | 0.12 [-] Show Supplier Material materials with Coefficient of friction of 0.12 [-] | DIN 53375, A, Against dry running steel |
Densidad | 0.96 g/cm³ Show Supplier Material materials with Densidad of 0.96 g/cm³ | max., ISO 1183 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 61 [-] Show Supplier Material materials with Dureza Shore D of 61 [-] | ISO 868 |
65 [-] Show Supplier Material materials with Dureza Shore D of 65 [-] | ISO 868 | |
Elongación | 200 % Show Supplier Material materials with Elongación of 200 % | min., ISO 527 |
Hardness, Ball Indentation | 30 MPa Show Supplier Material materials with Hardness, Ball Indentation of 30 MPa | min., ISO 2039-1 |
Límite elástico | 20 MPa Show Supplier Material materials with Límite elástico of 20 MPa | ISO 527 |
Módulo elástico | 0.7 GPa Show Supplier Material materials with Módulo elástico of 0.7 GPa | min., ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 80 kJ/m² | min., ISO 179 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Conductividad térmica | 0.41 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.41 W/(m·K) | DIN 52612 | |
Temperatura de fusión | 130 - 135 °C Show Supplier Material materials with Temperatura de fusión of 130 - 135 °C | ISO 3146 | |
Temperatura máx. de funcionamiento | 80 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 80 °C | Longterm | |
Long | |||
Short | |||
Inflamabilidad | HB UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Surface resistivity | 1e+09 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+09 Ω/sq | max., IEC 60243 |
Volume resistivity | 1e+06 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+06 Ω·cm | max., IEC 60243 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA, RoHS,REACH | |
UV resistance | Partly |