General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1 g/cm³ Show Supplier Material materials with Densidad of 1 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.7 % Show Supplier Material materials with Elongación of 6.7 % | ASTM D638 |
Módulo de flexión | 23.0 °C | 3.97 GPa Show Supplier Material materials with Módulo de flexión of 3.97 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 4.3 GPa Show Supplier Material materials with Módulo elástico of 4.3 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 139 MPa Show Supplier Material materials with Resistencia a la flexión of 139 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 109 MPa Show Supplier Material materials with Resistencia a la tracción of 109 MPa | ASTM D638 |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 29 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 29 kJ/m² | ISO 179 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 0.5 % Show Supplier Material materials with Contracción of 0.3 - 0.5 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal, Washing machine drum, Water pump parts, Water treatment components, Furniture parts. | |
Fillers | 20% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C, Moisture Content 0.02%, Dew Point -29°C |