General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.48 g/cm³ Show Supplier Material materials with Densidad of 1.48 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.1 % Show Supplier Material materials with Elongación of 1.1 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 217 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 217 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 11.87 GPa Show Supplier Material materials with Módulo de flexión of 11.87 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 13.56 GPa Show Supplier Material materials with Módulo elástico of 13.56 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 191 MPa Show Supplier Material materials with Resistencia a la flexión of 191 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 157 MPa Show Supplier Material materials with Resistencia a la tracción of 157 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 154 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Contracción of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal and Washing machine drum | |
Color | Natural, and custom colors | |
Fillers | 60% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C |