General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.4 % Show Supplier Material materials with Elongación of 3.4 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 109 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 109 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 7.11 GPa Show Supplier Material materials with Módulo de flexión of 7.11 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 38.49 GPa Show Supplier Material materials with Módulo elástico of 38.49 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 111.7 MPa Show Supplier Material materials with Resistencia a la flexión of 111.7 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 84 MPa Show Supplier Material materials with Resistencia a la tracción of 84 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Contracción of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Used for automotive interior decoration, power tools, sports equipment, lawnmowers and snow blowers, industrial parts, office equipment housings, etc . | |
Color | Natural, and custom colors | |
Fillers | 30% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 70 - 110 MPa, Melt Temperature 210 - 240 °C, Mould temperature 60 - 90 °C, Pre-drying 2- 4 hrs @ 80 - 95 °C, Moisture Content 0.01% |