General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 - 3 % Show Supplier Material materials with Elongación of 2 - 3 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 214 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 214 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 801 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 801 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 6.34 GPa Show Supplier Material materials with Módulo de flexión of 6.34 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 165 MPa Show Supplier Material materials with Resistencia a la flexión of 165 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 107 MPa Show Supplier Material materials with Resistencia a la tracción of 107 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 149 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 149 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Contracción of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Door module, Gear shifter basel, Engine under shield, Handle, Washing machine drum | |
Color | Natural | |
Fillers | 33% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C, Moisture Content 0.02%, Dew Point -29°C |