General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.5 - 2.5 % Show Supplier Material materials with Elongación of 1.5 - 2.5 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 294 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 294 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 961 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 961 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 10.34 GPa Show Supplier Material materials with Módulo de flexión of 10.34 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 11.72 GPa Show Supplier Material materials with Módulo elástico of 11.72 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 200 MPa Show Supplier Material materials with Resistencia a la flexión of 200 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 124 MPa Show Supplier Material materials with Resistencia a la tracción of 124 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 154 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Contracción of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Car handle, Car mirror parts, Battery case, Truck (SUV) outside pedal | |
Fillers | Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 191 - 232 °C, Mould temperature 32 - 66 °C, Pre-drying 2 hrs @ 79 °C |