General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 - 3 % Show Supplier Material materials with Elongación of 2 - 3 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 187 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 187 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1068 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1068 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 7.59 GPa Show Supplier Material materials with Módulo de flexión of 7.59 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 8.28 GPa Show Supplier Material materials with Módulo elástico of 8.28 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 203 MPa Show Supplier Material materials with Resistencia a la flexión of 203 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 128 MPa Show Supplier Material materials with Resistencia a la tracción of 128 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Contracción of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, power tool housing, high-speed rail accessories, Water pump impeller, Washing machine drum, Automotive: Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end | |
Color | White/Also as required | |
Fillers | 20% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 243 - 271 °C, Mould temperature 54 - 93 °C, Pre-drying 2 hrs @ 82 °C, Moisture Content 0.2%, Dew Point -29°C |