General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 - 3 % Show Supplier Material materials with Elongación of 2 - 3 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 187 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 187 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 801 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 801 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 9.65 GPa Show Supplier Material materials with Módulo de flexión of 9.65 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 10.34 GPa Show Supplier Material materials with Módulo elástico of 10.34 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 276 MPa Show Supplier Material materials with Resistencia a la flexión of 276 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la tracción of 179 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 249 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 249 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Contracción of 0.2 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Suitable for automotive (Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end), electronic appliances, sport equipment, power tools, tool handles, high speed rail accessories and etc. | |
Color | Natural/Also as required | |
Fillers | 33% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 277 - 299 °C, Mould temperature 66 - 107 °C, Pre-drying 4 hrs @ 79 °C, Moisture Content 0.2%, Dew Point -18°C |