General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 0.7 % Show Supplier Material materials with Elongación of 0.7 % | ASTM D638 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 726 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 726 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 25.39 GPa Show Supplier Material materials with Módulo de flexión of 25.39 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 37.89 GPa Show Supplier Material materials with Módulo elástico of 37.89 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 304 MPa Show Supplier Material materials with Resistencia a la flexión of 304 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 218 MPa Show Supplier Material materials with Resistencia a la tracción of 218 MPa | ASTM D638 |
Technological properties
Property | ||
---|---|---|
Application areas | Drone rack, Drone wing, 5G communication, Bone External Fixator bracket, Marine propellers. | |
Fillers | 40% Carbon Fiber | |
Processing methods | Injection Molding |