General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.53 g/cm³ Show Supplier Material materials with Densidad of 1.53 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 - 3 % Show Supplier Material materials with Elongación of 2 - 3 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 222 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 222 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 9656 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 9656 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 6.21 GPa Show Supplier Material materials with Módulo de flexión of 6.21 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 10.35 GPa Show Supplier Material materials with Módulo elástico of 10.35 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 221 MPa Show Supplier Material materials with Resistencia a la flexión of 221 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 204 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 204 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Contracción of 0.2 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Color | Natural, and custom colors | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 110 MPa, Melt Temperature 250 - 280 °C, Mould temperature 50 - 125 °C, Pre-drying 4 hrs @ 121 °C, Moisture Content 0.02% |