General
Property | Value |
---|---|
Bound AN Content | 28.0 % Show Supplier Material materials with Bound AN Content of 28.0 % |
Densidad | 0.98 g/cm³ Show Supplier Material materials with Densidad of 0.98 g/cm³ |
Volatile share | 0.3 % Show Supplier Material materials with Volatile share of 0.3 % |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongación | 510 % Show Supplier Material materials with Elongación of 510 % | ASTM D412 | 145°C×50min. Cured |
Módulo a elongación del 300 % | 0.02 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.02 GPa | ASTM D412 | 145°C×50min. Cured |
Resistencia a la tracción | 250 MPa Show Supplier Material materials with Resistencia a la tracción of 250 MPa | ASTM D412 | 145°C×50min. Cured |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Contenido de cenizas | 0.1 % Show Supplier Material materials with Contenido de cenizas of 0.1 % | max. |
Rheological Properties
Property | Value | Comment |
---|---|---|
Viscosidad mooney | 60 MU Show Supplier Material materials with Viscosidad mooney of 60 MU | ML1+4 and 100°C |
Technological properties
Property | ||
---|---|---|
Application areas | NBR 2860 is recommended for use in industrial and automotive parts such as packing, gasket and oil hose. | |
Color | Light Tan | |
Other | Shelf Life : 18 months from date of production atb room temperatures not exceeding 30°C under belowed storage condition (Retest critical parameters like MV and others after the expiry of shelf life). Storage condition: NBR should be stored in warehouse to be protected from sunlight, heat, moisture and foreign materials. | |
Packaging size | Bale Weight: 35kg Bale wrapping film: LDPE | |
Processing history | Polymerization: Cold Emulsion | |
Processing methods | Recipe (ASTM D3187): NBR 2860: 100 phr HAF(IRB #8): 40 ZnO: 3.0 Stearic Acid: 1.0 TBBS: 0.7 Sulfur: 1.5 Total: 146.2 | |
Stabilizer | Non-Staining |