General
Property | Value |
---|---|
Bound AN Content | 22.0 % Show Supplier Material materials with Bound AN Content of 22.0 % |
Densidad | 0.95 g/cm³ Show Supplier Material materials with Densidad of 0.95 g/cm³ |
Volatile share | 0.2 % Show Supplier Material materials with Volatile share of 0.2 % |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongación | 465 % Show Supplier Material materials with Elongación of 465 % | ASTM D412 | 145°C×50min. Cured |
Módulo a elongación del 300 % | 0.0155 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0155 GPa | ASTM D412 | 145°C×50min. Cured |
Resistencia a la tracción | 265 MPa Show Supplier Material materials with Resistencia a la tracción of 265 MPa | ASTM D412 | 145°C×50min. Cured |
Aplicaciones térmicas
Property | Value |
---|---|
Contenido de cenizas | 0.4 % Show Supplier Material materials with Contenido de cenizas of 0.4 % |
Rheological Properties
Property | Value | Comment |
---|---|---|
Viscosidad mooney | 55 MU Show Supplier Material materials with Viscosidad mooney of 55 MU | ML1+4 and 100°C (milled) |
Technological properties
Property | ||
---|---|---|
Application areas | NBR 2255 is preferably uesd for industrial belt, hoses, and many rubber parts such as seal and gasket. And also, it can be used for the industrial roller and low hardness roller of office printer due to good dynamic elasticity. | |
Color | Light Tan | |
Other | Shelf Life : 18 months from date of production atb room temperatures not exceeding 30°C under belowed storage condition (Retest critical parameters like MV and others after the expiry of shelf life). Storage condition: NBR should be stored in warehouse to be protected from sunlight, heat, moisture and foreign materials. | |
Packaging size | Bale Weight: 35kg Bale wrapping film: LDPE | |
Processing history | Polymerization: Cold Emulsion | |
Processing methods | Recipe (ASTM D3187): NBR 2255: 100 phr HAF(IRB #8): 40 ZnO: 3.0 Stearic Acid: 1.0 TBBS: 0.7 Sulfur: 1.5 Total: 146.2 | |
Stabilizer | Non-Staining |