General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 0.93 g/cm³ Show Supplier Material materials with Densidad of 0.93 g/cm³ | ISO 2781 | typical value |
0.95 g/cm³ Show Supplier Material materials with Densidad of 0.95 g/cm³ | ISO 2781 | typical value | |
Styrene content | 27 % Show Supplier Material materials with Styrene content of 27 % | LSY-QB-SD0151 (LG test) | typical value |
29 % Show Supplier Material materials with Styrene content of 29 % | LSY-QB-SD0151 (LG test) | typical value | |
Volatile share | 0.6 % Show Supplier Material materials with Volatile share of 0.6 % | ASTM D1416 | max. |
Mecánica
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Yellowness Index | 6 [-] Show Supplier Material materials with Yellowness Index of 6 [-] | ASTM D1925 | max. |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Asphalt Modifier | |
Packaging size | Paper bag(20kg), Flecon bag(500kg) |