General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Densidad of 1.55 g/cm³ | ASTM D792 |
Recycled Content | 45 % Show Supplier Material materials with Recycled Content of 45 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de flexión | 23.0 °C | 5.9 GPa Show Supplier Material materials with Módulo de flexión of 5.9 GPa | ISO 178, 2 mm/min |
Resistencia a la flexión | 23.0 °C | 150 MPa Show Supplier Material materials with Resistencia a la flexión of 150 MPa | ISO 178, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | ISO 527, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 15 % Show Supplier Material materials with Contenido de cenizas of 15 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ISO 75 | |||
Inflamabilidad | V0, V0 5VA for 3.2 mm sample UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 37 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 37 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Volume resistivity | 23.0 °C | 1.00E+18 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+18 Ω·cm | ASTM D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components, appliances and structral applications. | |
Certifications | RoHS,RECH | |
Color | Black | |
Fillers | 15% Glass Fiber and Mineral Powder | |
Processing methods |