General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de flexión | 23.0 °C | 6 GPa Show Supplier Material materials with Módulo de flexión of 6 GPa | ISO 178, 2 mm/min |
Resistencia a la flexión | 23.0 °C | 150 MPa Show Supplier Material materials with Resistencia a la flexión of 150 MPa | ISO 178, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | ISO 527, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180 |
Aplicaciones térmicas
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Automotive structural parts (e.g. sunroof frames). | |
Certifications | RoHS,RECH | |
Color | Black | |
Fillers | 15% Glass Fiber and Mineral Powder | |
Processing methods |