General
Property | Value |
---|---|
Recycled Content | 58 % Show Supplier Material materials with Recycled Content of 58 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 9.4 GPa Show Supplier Material materials with Módulo de flexión of 9.4 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 205 MPa Show Supplier Material materials with Resistencia a la flexión of 205 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 132 MPa Show Supplier Material materials with Resistencia a la tracción of 132 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Sunroof rails,Structural applications (e.g. grill retainers and lamp holders). | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Color | Black | |
Fillers | 30% Glass Fiber | |
Processing methods |