General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.87 g/cm³ Show Material materials with Densidad of 0.87 g/cm³ | ASTM D792 |
Viscosidad mooney | 23.0 °C | 36 MU Show Material materials with Viscosidad mooney of 36 MU | ASTM D1646 | ML 1+4, 121 °C |
Mecánica
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable,Impact modification |