Thermoplastic Polyolefin (TPO)
SABIC® PPcompound 8620AThermoplastic Polyolefin (TPO)
SABIC® PPcompound 8620Thermoplastic Polyolefin (TPO)
SABIC® PPcompound 9710Thermoplastic Polyolefin (TPO)
SABIC® PPcompound 8611AThermoplastic Polyolefin (TPO)
SABIC® PPcompound 9712Thermoplastic Polyolefin (TPO)
Olefinic thermoplastic elastomer (TPO)Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 101-35Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 101-55Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 101-64Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 101-73Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 101-80Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 101-87Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 103-40Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
EPDM/PP Deprene 103-50Suministrada por:
Lingen Plastic Rubber Co., Ltd.Thermoplastic Polyolefin (TPO)
SABIC® FORTIFY™ C0570DThermoplastic Polyolefin (TPO)
SABIC® FORTIFY™ C1055DThermoplastic Polyolefin (TPO)
SABIC® FORTIFY™ C1070Thermoplastic Polyolefin (TPO)
SABIC® FORTIFY™ C1070DThermoplastic Polyolefin (TPO)
SABIC® FORTIFY™ C1085Thermoplastic Polyolefin (TPO)
SABIC® FORTIFY™ C11075DF