General
Property | Value | Comment |
---|---|---|
Densidad | 0.868 g/cm³ Show Material materials with Densidad of 0.868 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Módulo de flexión | 0.0108 GPa Show Material materials with Módulo de flexión of 0.0108 GPa | ASTM D790 A | (1% Secant) |
Resistencia a desgarros | 35.3 kN/m Show Material materials with Resistencia a desgarros of 35.3 kN/m | ASTM D624 |
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Viscosidad mooney | 8.0 MU Show Material materials with Viscosidad mooney of 8.0 MU | ASTM D1646 | ML 1+4, 121 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Impact modification |