General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.95 g/cm³ Show Material materials with Densidad of 0.95 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 40 [-] Show Material materials with Dureza Shore D of 40 [-] | ISO 7619-1 | 15 seconds |
Elongación | 23.0 °C | 150 % Show Material materials with Elongación of 150 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.6 GPa Show Material materials with Módulo de flexión of 0.6 GPa | ISO 178 |
Resistencia a desgarros | 23.0 °C | 100 kN/m Show Material materials with Resistencia a desgarros of 100 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 16 MPa Show Material materials with Resistencia a la tracción of 16 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 65 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 65 kJ/m² | ISO 180/1A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.7 % Show Material materials with Contracción of 0.7 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 4 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 4 g/10min | ISO 1133 | 230°C/2.16kg | |
Velocidad de flujo del volumen derretido | 4.5 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 4.5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 65°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 230°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 35°C, Max. mold temperature: 50°C, Hold pressure range: as low as possible, Back pressure: 1MPa |