General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.89 g/cm³ Show Material materials with Densidad of 0.89 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 37 [-] Show Material materials with Dureza Shore D of 37 [-] | ISO 7619-1 | 15 seconds |
Elongación | 23.0 °C | 550 % Show Material materials with Elongación of 550 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.38 GPa Show Material materials with Módulo de flexión of 0.38 GPa | ISO 178 |
Resistencia a desgarros | 23.0 °C | 90 kN/m Show Material materials with Resistencia a desgarros of 90 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 12 MPa Show Material materials with Resistencia a la tracción of 12 MPa | ISO 527-1/-2 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Temperature: 65°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 225°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 30°C, Max. mold temperature: 50°C |