General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.88 g/cm³ Show Material materials with Densidad of 0.88 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 43 [-] Show Material materials with Dureza Shore D of 43 [-] | ISO 7619-1 | 15 seconds |
Elongación | 23.0 °C | 110 % Show Material materials with Elongación of 110 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.42 GPa Show Material materials with Módulo de flexión of 0.42 GPa | ISO 178 |
Resistencia a desgarros | 23.0 °C | 115 kN/m Show Material materials with Resistencia a desgarros of 115 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 19 MPa Show Material materials with Resistencia a la tracción of 19 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 58 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 58 kJ/m² | ISO 180/1A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.9 % Show Material materials with Contracción of 0.9 % | ISO 294-4, 2577 |
Velocidad de flujo del volumen derretido | 6 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 6 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: no, Melt Temperature Optimum: 260°C, Mold Temperature Optimum: 30°C, Min. mold temperature: 20°C, Max. mold temperature: 40°C, Hold pressure range: as low as possible, Back pressure: 1MPa |