General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Resistencia a la tracción | 325.0 MPa Show Material materials with Resistencia a la tracción of 325.0 MPa | Pink Sheets, ASTM B686 | Casting |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 100 °C | 963 J/(kg·K) Show Material materials with Calor específico of 963 J/(kg·K) | unstated value | ||
Coeficiente de dilatación térmica | 300 °C | 0.0000229 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000229 1/K | derived value for 20-300°C | ||
Conductividad térmica | 23 °C | 128 W/(m·K) Show Material materials with Conductividad térmica of 128 W/(m·K) | unstated value | ||
Temperatura de fusión | 546.0 - 621.0 °C Show Material materials with Temperatura de fusión of 546.0 - 621.0 °C | Pink Sheets, ASTM B686 | Casting |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Cobre | 1.6 - 2.0 % Show Material materials with Cobre of 1.6 - 2.0 % | Pink Sheets, ASTM B686 | Casting |
Hierro | 0.20 % Show Material materials with Hierro of 0.20 % | Pink Sheets, ASTM B686 | Casting |
Magnesio | 0.4 - 0.6 % Show Material materials with Magnesio of 0.4 - 0.6 % | Pink Sheets, ASTM B686 | Casting |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | Pink Sheets, ASTM B686 | Casting |
Silicona | 8.6 - 9.4 % Show Material materials with Silicona of 8.6 - 9.4 % | Pink Sheets, ASTM B686 | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | Pink Sheets, ASTM B686 | Casting |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | Pink Sheets, ASTM B686 | Casting |