General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium |
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 100 °C | 963 J/(kg·K) Show Material materials with Calor específico of 963 J/(kg·K) | unstated value |
Coeficiente de dilatación térmica | 100 °C | 0.0000209 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000209 1/K | nominal value between 20°C and the mentioned temperature |
300 °C | 0.0000229 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000229 1/K | nominal value between 20°C and the mentioned temperature | |
Conductividad térmica | 25 °C | 113 W/(m·K) Show Material materials with Conductividad térmica of 113 W/(m·K) | unstated value |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |