Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 12 - 18 % Show Material materials with Elongación of 12 - 18 % |
Límite elástico | 23.0 °C | 210 - 270 MPa Show Material materials with Límite elástico of 210 - 270 MPa |
Resistencia a la tracción | 23.0 °C | 440 - 460 MPa Show Material materials with Resistencia a la tracción of 440 - 460 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 1 % Show Material materials with Aluminio of 1 % |
Cobre | 58 % Show Material materials with Cobre of 58 % |
Estaño | 0.6 % Show Material materials with Estaño of 0.6 % |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Zinc | 39 % Show Material materials with Zinc of 39 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware and fasteners;Other: Gas valves and fittings, fasteners, pump trim, gears, locks, heavy-duty electrical connectors, transmission components, safety tools and decorative metalwork | |
Corrosion properties | Good corrosion resistance | |
General machinability | Good machinability |