BS CZ126 (CW707R) Arsenical Brass

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

CZ126 (CW707R) is an arsenical brass available in tubular form. It contains 70% copper 30% zinc with a small addition of arsenic, which improves the corrosion resistance without affecting the ductility and forming characteristics of the material. With reasonable strength levels this alloy is utilised in heat exchangers, condensers and in other components requiring general purpose tube. This material offers a good workability and can be manipulated by a number of techniques. It also lends itself to soldering and brazing.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Mecánica

PropertyTemperatureValue

Dureza Vickers

23.0 °C

130 [-]

Show Material materials with Dureza Vickers of 130 [-]

Resistencia a la tracción

23.0 °C

400 MPa

Show Material materials with Resistencia a la tracción of 400 MPa

Chemical properties

PropertyValue

Arsénico

0.04 %

Show Material materials with Arsénico of 0.04 %

Cobre

70 %

Show Material materials with Cobre of 70 %

Zinc

30 %

Show Material materials with Zinc of 30 %

Technological properties

Property
Application areas

Chemical processing: Heat exchangers and condensers

Corrosion properties

With an addition of arsenic that improves the corrosion resistance

General machinability

Good machining