Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 22 - 28 % Show Material materials with Elongación of 22 - 28 % |
Resistencia a la tracción | 23.0 °C | 330 - 350 MPa Show Material materials with Resistencia a la tracción of 330 - 350 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General: Nuts, rivets, screws, instrument parts, clock and watch components, battery terminals and other parts requiring good machinability with a limited amount of cold forming | |
Cold Forming | Reasonable cold forming | |
Corrosion properties | Reasonable corrosion resistance | |
General machinability | Good machining |