Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 25 - 28 % Show Material materials with Elongación of 25 - 28 % |
Resistencia a la tracción | 23.0 °C | 350 - 380 MPa Show Material materials with Resistencia a la tracción of 350 - 380 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General: Hot forged components, condenser and heat exchanger tubeplates, fasteners, pothole windows, decorative brassware, extruded sections and items that require blanking or limited bending | |
Cold Forming | Limited cold forming | |
Corrosion properties | Good corrosion resistance | |
General machinability | Good machining | |
Hot forming | Good hot foming |