General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.53 g/cm³ Show Material materials with Densidad of 8.53 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 75 - 95 [-] Show Material materials with Dureza Brinell of 75 - 95 [-] |
Elongación | 23.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 260 MPa Show Material materials with Límite elástico Rp 0,2 of 260 MPa |
Módulo elástico | 23.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa |
Resistencia a la tracción | 23.0 °C | 485 MPa Show Material materials with Resistencia a la tracción of 485 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 36 W/(m·K) Show Material materials with Conductividad térmica of 36 W/(m·K) |
Temperatura de fusión | 970 - 1025 °C Show Material materials with Temperatura de fusión of 970 - 1025 °C |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobre | Balance | ||
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % | max. | |
Manganeso | 0.5 - 1.3 % Show Material materials with Manganeso of 0.5 - 1.3 % | ||
Silicona | 2.8 - 3.8 % Show Material materials with Silicona of 2.8 - 3.8 % | ||
Zinc | 1.5 % Show Material materials with Zinc of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Architectural & decorative: Furniture, fire place surrounds, nameplates, sculptures, signs, bolts, cladding, door and window frames, hinge pins, latches, masonry fixings, slate and tile nails, panels, spring brackets, screws, step irons, tension bolts and wall ties;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings, heavy-duty switchgear, bearing plates, bolts, busbar clamps, bushes, clutch discs, cotter pins, electrical conduit, fasteners, locking washers, piston rings, thrust washers and u-bolts;Automotive: valve guides, bushes and valve seats;Chemical processing: Autoclaves, chemical apparatus, drains, explosives plant, fans and ducts for corrosive vapours, fasteners, heat exchanger tube plates, filters, pickling and recovery plant, pressure vessels, pump rods and shafts, screen plates, stirrers, valve stems, vats and washers;Offshore & marine: Fasteners, propeller shafts, hull and deck fittings, fuel and water tanks, non-magnetic instrumentation, subsea electromechanical equipment and other hardware | |
Cold Forming | Excellent cold formability | |
Corrosion properties | Excellent corrosion resistance | |
Hot forming | Excellent hort formability, Hot Working Temperature (°C): 710-870 |