General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.44 g/cm³ Show Material materials with Densidad of 8.44 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 23.0 °C | 275 - 415 MPa Show Material materials with Límite elástico Rp 0,2 of 275 - 415 MPa |
Módulo elástico | 23.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa |
Resistencia a la tracción | 23.0 °C | 690 - 830 MPa Show Material materials with Resistencia a la tracción of 690 - 830 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.28E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.28E-5 1/K | for 0-100°C |
Conductividad térmica | 23.0 °C | 9.8 W/(m·K) Show Material materials with Conductividad térmica of 9.8 W/(m·K) | |
Temperatura de fusión | 1290 - 1350 °C Show Material materials with Temperatura de fusión of 1290 - 1350 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.32E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.32E-6 Ω·m |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % | |
Cromo | 22 % Show Material materials with Cromo of 22 % | |
Hierro | 2 % Show Material materials with Hierro of 2 % | |
Molibdeno | 9 % Show Material materials with Molibdeno of 9 % | |
Niobio | 3.5 % Show Material materials with Niobio of 3.5 % | Nb+Ta |
Níquel | 58 - 61 % Show Material materials with Níquel of 58 - 61 % | |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | |
Tántalo | 3.5 % Show Material materials with Tántalo of 3.5 % | Nb+Ta |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Components where exposure to sea water and high mechanical stresses are required, oil and gas production where hydrogen sulphide and elementary sulphur exist at temperature in excess of 150C, flare stacks, hydrocarbon processing from tar-sand and oil-shale recovery projects;Chemical processing: Flue gas desulphurisation plant, flare stacks, offshore sour oil and gas production, waste incineration, phosphoric acid production and nuclear fuel processing | |
Corrosion properties | Very good corrosion resistance |