General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | |
Dureza Brinell | 23.0 °C | 270 [-] Show Material materials with Dureza Brinell of 270 [-] | max. |
Elongación | 23.0 °C | 25 % Show Material materials with Elongación of 25 % | |
Límite elástico Rp 0,2 | 23.0 °C | 448 MPa Show Material materials with Límite elástico Rp 0,2 of 448 MPa | |
Módulo de cizallamiento | 23.0 °C | 75 GPa Show Material materials with Módulo de cizallamiento of 75 GPa | |
Módulo elástico | 23.0 °C | 199 GPa Show Material materials with Módulo elástico of 199 GPa | |
Resistencia a la tracción | 23.0 °C | 620 MPa Show Material materials with Resistencia a la tracción of 620 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 425 J/(kg·K) Show Material materials with Calor específico of 425 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.11E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11E-5 1/K | for 20-100°C |
Conductividad térmica | 23.0 °C | 14 W/(m·K) Show Material materials with Conductividad térmica of 14 W/(m·K) | for 20-300°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 8E-7 Ω·m Show Material materials with Resistividad eléctrica of 8E-7 Ω·m |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 33 [-] Show Material materials with Permeabilidad magnética relativa of 33 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % | max. | |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % | max. | |
Cromo | 21 - 23 % Show Material materials with Cromo of 21 - 23 % | ||
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | max. | |
Hierro | Balance | ||
Manganeso | 2 % Show Material materials with Manganeso of 2 % | max. | |
Molibdeno | 2.5 - 3.5 % Show Material materials with Molibdeno of 2.5 - 3.5 % | ||
Nitrógeno | 0.08 - 0.2 % Show Material materials with Nitrógeno of 0.08 - 0.2 % | ||
Níquel | 4.5 - 6.5 % Show Material materials with Níquel of 4.5 - 6.5 % | ||
Silicona | 1 % Show Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Offshore pipework, components for gas, oil and process cooling plants, wellhead and subsea wellhead fittings, desalination plant, seawater cooled heat exchangers and high strength fasteners;Chemical processing: Chemical tanks, flue gas filters, acetic acid distillation parts and heat exchangers | |
Corrosion properties | Very good corrosion resistance | |
General machinability | Good workability |