Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 280 [-] Show Material materials with Dureza Brinell of 280 [-] | max. |
Elongación | 23.0 °C | 15 % Show Material materials with Elongación of 15 % | |
Límite elástico | 23.0 °C | 315 - 550 MPa Show Material materials with Límite elástico of 315 - 550 MPa | |
Resistencia a la tracción | 23.0 °C | 760 - 800 MPa Show Material materials with Resistencia a la tracción of 760 - 800 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Offshore platforms and equipment, components for gas, oil and process cooling plants, wellhead and subsea wellhead fittings, desalination plants, seawater cooled heat exchangers and high strength fasteners;Chemical processing: Chemical tanks, flue gas filters, acid distillation components and heat exchangers | |
Corrosion properties | Very good corrosion resistance | |
General machinability | Good workability |