Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
17-4PH Stainless Steel
1.4542 (X5CrNiCuNb16-4) is a well-established precipitation hardening martensitic stainless steel capable of achieving very high strength and hardness after a relatively simple heat treatment. It offers excellent corrosion resistance combined with a structured range of mechanical property levels depending on the precise heat treatment applied. It is readily machined and fabricated in the softer tempers and can then be heat-treated to exceptional strength and dimensional stability. It shows the following features and properties:
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Suppliers with similar grades
Healthcare
Equipos médicos
Medical Equipment General
Sistemas mecánicos
Elementos de sujeción
Aeroespacial
Fijadores para el sector aeroespacial
Pernos
Tornillos
Anillos
Piezas de desgaste
Automotriz
Sistemas para vehículos de carretera
Acoplamientos
Construcción
Elementos de construcción
Ejes
Muelles
Piezas generales para vehículos
Engranajes
Válvulas
Sistemas de fluido
Valve Spindle
Sistemas de energía fluida
Bombas y motores
Fabricación
Mecanización
Milling Machines
Corte
Milling Tools
Energía
Energía nuclear
Other Standards Related To Nuclear Energy
Marítimo
Estructuras navales y construcción de barcos
General Ship Building & Marine Structures
Boats
Bearings For Aerospace
Aerospace Fittings
Estructuras aeroespaciales
Motores y propulsión aeroespacial
Turbine
Industria química
Producción de industria química
Industria del papel
Equipment For The Paper Industry
Defensa
Ingeniería militar
4130 Steel (Chromoly): Properties and Applications
440C Stainless Steel: Properties, Processing and Application
7Cr17MoV vs 7Cr17 Stainless Steel
A Guide to Rebar Sizes – an overview of steel reinforcement bars
AISI 304 (1.4301) Stainless Steel
AISI 316 Stainless Steel: Specification and Datasheet
ASTM A1018
ASTM A108 Carbon and Alloy Steel Bars
ASTM A479 Stainless Steel
ASTM A53 Carbon Steel Pipes
ASTM A564 Stainless Steel Age Hardened
Advanced High Strength Steel: Nomenclature, Grades, and Applications
Alloy Steel: Properties, Processing and Applications
Austenitic Stainless Steel: Properties, Applications and Grades
Carbon Steel: Properties, Production, Examples and Applications
Cold Rolled Steels
Difference between AISI 316, AISI 316L and AISI 316LN Stainless Steel
Duplex Stainless Steel: Properties, Standards, and Applications
Electrical Steel: Properties, Types, Production, and Applications
Ferritic Stainless Steel: Properties, Grades, and Applications
Hot Rolled Steels
Introduction to Steel Grades
JIS SCM435 equivalent materials
Machinability, Castability, Formability, Hardenability and Weldability of Steel
Maraging Steel: Properties, Processing, and Applications
Martensitic Stainless Steel: Properties, Grades, and Applications
Materials Used in Bearings
Materials Used in Bridges
Precipitation Hardening (Age Hardening)
SUS304 Stainless Steel vs SS304: What’s the Difference?
Stainless Steel: Properties, Production, Examples and Applications
Top Stainless Steel Suppliers in Europe
What is ASTM A182 Grade F6a Stainless Steel?
What is ASTM A36?
What is ASTM A53?
What is EN 10025 Grade S235JR?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value | Comment | |
---|---|---|---|
Cobre | 4 % Show Material materials with Cobre of 4 % | ||
Cromo | 17 % Show Material materials with Cromo of 17 % | ||
Hierro | Balance | ||
Niobio | 0.3 % Show Material materials with Niobio of 0.3 % | Nb+Ta | |
Níquel | 4 % Show Material materials with Níquel of 4 % | ||
Tántalo | 0.3 % Show Material materials with Tántalo of 0.3 % | Nb+Ta |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Offshore foils, helicopter deck platforms, pump shafts, couplings, fasteners, valve parts and spindles;Aerospace: Turbine blades, missile and rocket fittings, undercarriage components and fasteners;Other: Nuclear waste casks, medical instruments, paper mill equipment and chemical process plant, springs, screws, bolts, gears, bushes and wear rings | |
Corrosion properties | Very high corrosion resistance | |
General machinability | It is readily machinable |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.