General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.43 g/cm³ Show Material materials with Densidad of 4.43 g/cm³ | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Mecánica
Property | Value | Related Standards | Shape |
---|---|---|---|
Dureza Rockwell C | 36 [-] Show Material materials with Dureza Rockwell C of 36 [-] | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Elongación | 10 % Show Material materials with Elongación of 10 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Módulo elástico | 114.0 GPa Show Material materials with Módulo elástico of 114.0 GPa | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Resistencia a la tracción | 895.0 - 931.0 MPa Show Material materials with Resistencia a la tracción of 895.0 - 931.0 MPa | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Aplicaciones térmicas
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Calor específico | 370.0 - 674.0 J/(kg·K) Show Material materials with Calor específico of 370.0 - 674.0 J/(kg·K) | Typical for Titanium Alpha Beta Alloy | ||
Coeficiente de dilatación térmica | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Conductividad térmica | 6.7 W/(m·K) Show Material materials with Conductividad térmica of 6.7 W/(m·K) | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar | |
Temperatura de fusión | 1674 °C Show Material materials with Temperatura de fusión of 1674 °C | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Eléctrico
Property | Value | Related Standards | Shape |
---|---|---|---|
Resistividad eléctrica | 1.8000000000000001e-06 Ω·m Show Material materials with Resistividad eléctrica of 1.8000000000000001e-06 Ω·m | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 5.5 - 6.75 % Show Material materials with Aluminio of 5.5 - 6.75 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Hidrógeno | 0.0125 % Show Material materials with Hidrógeno of 0.0125 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Nitrógeno | 0.05 % Show Material materials with Nitrógeno of 0.05 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Oxígeno | 0.2 % Show Material materials with Oxígeno of 0.2 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Vanadio | 3.5 - 4.5 % Show Material materials with Vanadio of 3.5 - 4.5 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Compressor blades, discs and rings for jet engines, airframe components, fasteners, rocket engine cases, helicopter rotor blades and critical forgings;Offshore & marine: Offshore tubulars and oil and gas equipment;Other: Biomedical implants and chemical processing equipment | |
Corrosion properties | Good corrosion resistance |