General
Property | Value | Shape |
---|---|---|
Densidad | 4.65 g/cm³ Show Material materials with Densidad of 4.65 g/cm³ | Bar, Billet |
Medidas
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Diámetro | 7 mm Show Material materials with Diámetro of 7 mm | Bar | ||
115 mm Show Material materials with Diámetro of 115 mm | Bar | |||
130 mm Show Material materials with Diámetro of 130 mm | Billet | |||
350 mm Show Material materials with Diámetro of 350 mm | Billet | |||
Longitud | 3000 mm Show Material materials with Longitud of 3000 mm | Billet | ||
4500 mm Show Material materials with Longitud of 4500 mm | Billet | |||
6000 mm Show Material materials with Longitud of 6000 mm | Bar | max |
Mecánica
Property | Value | Shape |
---|---|---|
Dureza Brinell | 304.0 Show Material materials with Dureza Brinell of 304.0 | Bar, Billet |
Dureza Rockwell C | 32.0 [-] Show Material materials with Dureza Rockwell C of 32.0 [-] | Bar, Billet |
Dureza Vickers | 318.0 Show Material materials with Dureza Vickers of 318.0 | Bar, Billet |
Elongación | 9.0 % Show Material materials with Elongación of 9.0 % | Bar, Billet |
Límite elástico | 900.0 MPa Show Material materials with Límite elástico of 900.0 MPa | Bar, Billet |
Módulo de cizallamiento | 41.0 GPa Show Material materials with Módulo de cizallamiento of 41.0 GPa | Bar, Billet |
Módulo elástico | 110.0 Show Material materials with Módulo elástico of 110.0 | Bar, Billet |
Resistencia a la tracción | 970.0 MPa Show Material materials with Resistencia a la tracción of 970.0 MPa | Bar, Billet |
Aplicaciones térmicas
Property | Value | Shape | Comment |
---|---|---|---|
Calor específico | 490.0 - 580.0 J/(kg·K) Show Material materials with Calor específico of 490.0 - 580.0 J/(kg·K) | Typical for Titanium Beta Alloy | |
Coeficiente de dilatación térmica | 7.099999999999997e-06 - 9.699999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 7.099999999999997e-06 - 9.699999999999999e-06 1/K | Typical for Titanium Beta Alloy | |
Conductividad térmica | 7.8 W/(m·K) Show Material materials with Conductividad térmica of 7.8 W/(m·K) | Bar, Billet | |
Temperatura de fusión | 1550.0 - 1815.0 °C Show Material materials with Temperatura de fusión of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminio | 2.6 - 3.4 % Show Material materials with Aluminio of 2.6 - 3.4 % | Bar, Billet |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % | Bar, Billet |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | Bar, Billet |
Hierro | 1.6 - 2.2 % Show Material materials with Hierro of 1.6 - 2.2 % | Bar, Billet |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Bar, Billet |
Oxígeno | 0.13 Show Material materials with Oxígeno of 0.13 | Bar, Billet |
Vanadio | 9.0 - 11.0 % Show Material materials with Vanadio of 9.0 - 11.0 % | Bar, Billet |