General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.51 g/cm³ Show Material materials with Densidad of 4.51 g/cm³ | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Medidas
Property | Value | Related Standards | Shape |
---|---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | ASTM B-265, DIN 17860 | Sheet |
600 mm Show Material materials with Ancho of 600 mm | ASTM B-265, DIN 17860 | Plate | |
1524 mm Show Material materials with Ancho of 1524 mm | ASTM B-265, DIN 17860 | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | ASTM B-265, DIN 17860 | Plate | |
Diámetro | 5 mm Show Material materials with Diámetro of 5 mm | ASTM B-265, DIN 17860 | Tube |
12.7 mm Show Material materials with Diámetro of 12.7 mm | ASTM B-265, DIN 17860 | Tube | |
25.4 mm Show Material materials with Diámetro of 25.4 mm | ASTM B-265, DIN 17860 | Billet | |
38.1 mm Show Material materials with Diámetro of 38.1 mm | ASTM B-265, DIN 17860 | Tube | |
125 mm Show Material materials with Diámetro of 125 mm | ASTM B-265, DIN 17860 | Billet | |
130 mm Show Material materials with Diámetro of 130 mm | ASTM B-265, DIN 17860 | Tube | |
Longitud | 1000 mm Show Material materials with Longitud of 1000 mm | ASTM B-265, DIN 17860 | Tube |
1500 mm Show Material materials with Longitud of 1500 mm | ASTM B-265, DIN 17860 | Sheet, Plate | |
5000 mm Show Material materials with Longitud of 5000 mm | ASTM B-265, DIN 17860 | Sheet, Tube | |
6500 mm Show Material materials with Longitud of 6500 mm | ASTM B-265, DIN 17860 | Plate | |
20000 mm Show Material materials with Longitud of 20000 mm | ASTM B-265, DIN 17860 | Tube | |
Wall thickness | 0.4 - 1.65 mm Show Material materials with Wall thickness of 0.4 - 1.65 mm | ASTM B-265, DIN 17860 | Tube |
0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | ASTM B-265, DIN 17860 | Tube | |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | ASTM B-265, DIN 17860 | Billet |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.361 [-] Show Material materials with Coeficiente de Poisson of 0.361 [-] | Typical for Pure Titanium | ||
Dureza Brinell | 120.0 Show Material materials with Dureza Brinell of 120.0 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Elongación | 22.0 % Show Material materials with Elongación of 22.0 % | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Límite elástico | 170.0 MPa Show Material materials with Límite elástico of 170.0 MPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Typical for Pure Titanium | ||
Módulo elástico | 105.0 GPa Show Material materials with Módulo elástico of 105.0 GPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Resistencia a la tracción | 240.0 MPa Show Material materials with Resistencia a la tracción of 240.0 MPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Aplicaciones térmicas
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Calor específico | 520 J/(kg·K) Show Material materials with Calor específico of 520 J/(kg·K) | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Conductividad térmica | 21 W/(m·K) Show Material materials with Conductividad térmica of 21 W/(m·K) | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Temperatura de fusión | 1670.0 °C Show Material materials with Temperatura de fusión of 1670.0 °C | Typical for Pure Titanium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbono | 0.08 Show Material materials with Carbono of 0.08 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Hierro | 0.2 Show Material materials with Hierro of 0.2 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Nitrógeno | 0.03 Show Material materials with Nitrógeno of 0.03 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Oxígeno | 0.18 Show Material materials with Oxígeno of 0.18 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |