General
Property | Value |
---|---|
Densidad | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ |
Mecánica
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |||
Elongación | 20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | EN 573-3 | Plate | A50 |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | EN 573-3 | Plate | A50 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | EN 573-3 | Plate | A50 | |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | EN 573-3 | Plate | A50 | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | EN 573-3 | Plate | ||
Límite elástico | 40.0 MPa Show Material materials with Límite elástico of 40.0 MPa | ||||
20.0 °C | 75.0 MPa Show Material materials with Límite elástico of 75.0 MPa | EN 573-3 | Plate | RP02 | |
Módulo de cizallamiento | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |||
Módulo elástico | 67.0 GPa Show Material materials with Módulo elástico of 67.0 GPa | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |||
Resistencia a la tracción | 80.0 MPa Show Material materials with Resistencia a la tracción of 80.0 MPa | ||||
20.0 °C | 105.0 - 145.0 MPa Show Material materials with Resistencia a la tracción of 105.0 - 145.0 MPa | EN 573-3 | Plate |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 897.0 J/(kg·K) Show Material materials with Calor específico of 897.0 J/(kg·K) | |
Coeficiente de dilatación térmica | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | |
Conductividad térmica | 221.0 W/(m·K) Show Material materials with Conductividad térmica of 221.0 W/(m·K) | |
Temperatura de fusión | 645.0 - 660.0 °C Show Material materials with Temperatura de fusión of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 33000000.0 - 38000000.0 S/m Show Material materials with Conductividad eléctrica of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Resistividad eléctrica | 2.7e-08 - 3e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Boro | 0.05 Show Material materials with Boro of 0.05 | EN 573-3 | |
Cobre | 0.02 Show Material materials with Cobre of 0.02 | EN 573-3 | |
0.05 Show Material materials with Cobre of 0.05 | EN 573-3 | Plate | |
Cromo | 0.01 Show Material materials with Cromo of 0.01 | EN 573-3 | |
Galio | 0.03 Show Material materials with Galio of 0.03 | EN 573-3 | |
Hierro | 0.4 Show Material materials with Hierro of 0.4 | EN 573-3 | Plate |
Magnesio | 0.05 Show Material materials with Magnesio of 0.05 | EN 573-3 | Plate |
Manganeso | 0.01 Show Material materials with Manganeso of 0.01 | EN 573-3 | |
0.05 Show Material materials with Manganeso of 0.05 | EN 573-3 | Plate | |
Silicona | 0.1 Show Material materials with Silicona of 0.1 | EN 573-3 | |
0.25 Show Material materials with Silicona of 0.25 | EN 573-3 | Plate | |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | EN 573-3 | Plate |
0.1 - 0.2 % Show Material materials with Titanio of 0.1 - 0.2 % | EN 573-3 | ||
Zinc | 0.05 Show Material materials with Zinc of 0.05 | EN 573-3 | |
0.07 Show Material materials with Zinc of 0.07 | EN 573-3 | Plate |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |