General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | EN 573-3 | Strip, Sheet, Plate |
2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 4000 Series Aluminium |
Límite elástico | 70.0 MPa Show Material materials with Límite elástico of 70.0 MPa | |
Módulo de cizallamiento | 26.0 GPa Show Material materials with Módulo de cizallamiento of 26.0 GPa | Typical for Wrought 4000 Series Aluminium |
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium |
Resistencia a la tracción | 110.0 MPa Show Material materials with Resistencia a la tracción of 110.0 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Calor específico | 890.0 J/(kg·K) Show Material materials with Calor específico of 890.0 J/(kg·K) | |||
Coeficiente de dilatación térmica | 2.1600000000000003e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1600000000000003e-05 1/K | |||
20 °C | 2.16e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.16e-05 1/K | EN 573-3 | Strip, Sheet, Plate | |
100 °C | 2.16e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.16e-05 1/K | EN 573-3 | Strip, Sheet, Plate | |
Conductividad térmica | 180 W/(m·K) Show Material materials with Conductividad térmica of 180 W/(m·K) | EN 573-3 | Strip, Sheet, Plate | |
180.0 W/(m·K) Show Material materials with Conductividad térmica of 180.0 W/(m·K) | ||||
Temperatura de fusión | 575.0 - 615.0 °C Show Material materials with Temperatura de fusión of 575.0 - 615.0 °C | EN 573-3 | Strip, Sheet, Plate |
Eléctrico
Property | Value | Related Standards | Shape |
---|---|---|---|
Conductividad eléctrica | 27000000.0 S/m Show Material materials with Conductividad eléctrica of 27000000.0 S/m | EN 573-3 | Strip, Sheet, Plate |
Resistividad eléctrica | 3.7e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.7e-08 Ω·m | EN 573-3 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % | EN 573-3 | Strip, Sheet, Plate |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % | EN 573-3 | |
0.80 % Show Material materials with Hierro of 0.80 % | EN 573-3 | Strip, Sheet, Plate | |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | EN 573-3 | Strip, Sheet, Plate |
Silicona | 6.8 - 8.2 % Show Material materials with Silicona of 6.8 - 8.2 % | EN 573-3 | Strip, Sheet, Plate |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | EN 573-3 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |