General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.02 g/cm³ Show Material materials with Densidad of 8.02 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Estricción | 20.0 °C | 51 % Show Material materials with Estricción of 51 % | |
650.0 °C | 41 % Show Material materials with Estricción of 41 % | ||
760.0 °C | 50 % Show Material materials with Estricción of 50 % | ||
Límite elástico | 20.0 °C | 470 MPa Show Material materials with Límite elástico of 470 MPa | |
650.0 °C | 230 MPa Show Material materials with Límite elástico of 230 MPa | ||
760.0 °C | 170 MPa Show Material materials with Límite elástico of 170 MPa | ||
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 880 MPa Show Material materials with Resistencia a la tracción of 880 MPa | |
650.0 °C | 52 MPa Show Material materials with Resistencia a la tracción of 52 MPa | ||
760.0 °C | 320 MPa Show Material materials with Resistencia a la tracción of 320 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 760.0 °C | 1.93E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.93E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 0.35 - 0.5 % Show Material materials with Carbono of 0.35 - 0.5 % | |
Cromo | 12 - 15 % Show Material materials with Cromo of 12 - 15 % | |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % | |
Hierro | 64.2 - 73.65 % Show Material materials with Hierro of 64.2 - 73.65 % | Balance |
Manganeso | 1 % Show Material materials with Manganeso of 1 % | |
Molibdeno | 0.2 - 0.5 % Show Material materials with Molibdeno of 0.2 - 0.5 % | |
Níquel | 12 - 15 % Show Material materials with Níquel of 12 - 15 % | |
Silicona | 0.3 - 0.8 % Show Material materials with Silicona of 0.3 - 0.8 % | |
Wolframio | 1.5 - 3 % Show Material materials with Wolframio of 1.5 - 3 % |