Acero bajo en carbono
EN 10025-2 Grade S275J2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10025-2 Grade S275JR normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10025-2 Grade S235J0 normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10025-2 Grade S275J0 normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-3 Grade S460N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QH quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B534 Grade C17500 TD04Acero inoxidable endurecido por precipitación
Acidur 4542 P800Suministrada por:
Deutsche Edelstahlwerke (DEW)