General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.4 - 7.7 g/cm³ Show Material materials with Densidad of 7.4 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Dureza Brinell | 20.0 °C | 293 [-] Show Material materials with Dureza Brinell of 293 [-] | |
Elongación A5 | 20.0 °C | 8 - 15.5 % Show Material materials with Elongación A5 of 8 - 15.5 % | |
Estricción | 20.0 °C | 9 - 10 % Show Material materials with Estricción of 9 - 10 % | |
Límite elástico | 20.0 °C | 840 - 844 MPa Show Material materials with Límite elástico of 840 - 844 MPa | |
Módulo elástico | 20.0 °C | 194 - 220 GPa Show Material materials with Módulo elástico of 194 - 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 940 - 941 MPa Show Material materials with Resistencia a la tracción of 940 - 941 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 200.0 °C | 9.8E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 9.8E-6 1/K | The mentioned values are between 20°C and the mentioned temperature |
600.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.24E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.24E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.31E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.31E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.75 - 0.9 % Show Material materials with Carbono of 0.75 - 0.9 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 0.8 % Show Material materials with Manganeso of 0.8 % |
Níquel | 1 - 1.7 % Show Material materials with Níquel of 1 - 1.7 % |
Silicona | 1.75 - 2.6 % Show Material materials with Silicona of 1.75 - 2.6 % |