Densidad: 7.4 - 7.7 g/cm³

Quick Comparison

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Suministrada por:

1 proveedor Matmatch

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Acero inoxidable martensítico

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Suministrada por:

1 proveedor Matmatch

Acero inoxidable ferrítico

Sandvik 4C54

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Acero inoxidable ferrítico

UGIMA® 4511 Work Hardened (drawn)

Suministrada por:

Ugitech

Wrought Copper Bronze Aluminium Bronze

AMPCO® 45 Extruded and drawn rods

Suministrada por:

AMPCO METAL

Acero inoxidable martensítico

Corrodur 4021 QT800

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

Corrodur 4034 Annealed

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

Acidur 4057 QT800

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

Acidur 4418 QT900

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

Corrodur 4021 QT700

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

Acidur 4057 QT900

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

Acidur 4418 QT760

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch